Tsarin smome corundum iri ɗaya ne da farin dutsen fari, sai dai cewa an ƙara wasu adadin Chrome oxide, wanda yake launin shuɗi ko launin shuɗi. Kamfanin CHromium saboda gabatarwar CR3, + Inganta wahalar fargaba, da taurin kai tana da matukar farin ciki, da kuma kusa da babban aiki da kuma kayan aikin Chromium, wanda ya dace da kayan aiki ya zama mafi girman kayan aiki da kayan aikin cromplic. kayan tarihi.
1, Chrome Cigangum ne aluminum kayan oxide foda kamar yadda babban albarkatun kasa, wanda aka daidaita da oromium oxide, ta babban zazzabi Arc farun faranti.
2, launi mai ruwan hoda ne, tuƙin yayi kama da fararen fata, yana da tauri ya fi dutsen fari. Abrasivais da aka kera ta da kyawawan dorewa da kuma girma nika gama.
3, dace da kayan aikin auna, kayan aikin kayan aiki spindle, sassan kayan aiki, zaren kayan aiki wanda yake nika da sauran madaidaici.
Ruwan hoda mai ban sha'awa da aka haife shiGritMuhawara | |
Raga | Matsakaicin rauni Karamin lambar raga, da mai kula da grit |
8 raga | 45% 8 raga (2.3 mm) ko girma |
10 raga | 45% 10 raga (2.0 mm) ko girma |
12 raga | 45% 12 raga (1.7 mm) ko girma |
14 raga | 45% 14 raga (1.4 mm) ko girma |
16 raga | 45% 16 raga (1.2 mm) ko girma |
20 ISH | 70% 20 raga (0.85 mm) ko girma |
22 raga | 45% 20 raga (0.85 mm) ko girma |
24 Mesh | 45% 25 Mesh (0.7 mm) ko girma |
30 ISH | 45% 30 raga (0.56 mm) ko girma |
36 raga | 45% 35 raga (0.48 mm) ko girma |
40 raga | 45% 40 MIsh (0.42 mm) ko girma |
46 raga | 40% raga (0.35 mm) ko mafi girma |
54 raga | 40% 50 raga (0.33 mm) ko girma |
60 raga | 40% miliyan 60 (0.25 mm) ko girma |
70 raga | 45% 70 raga (0.21 mm) ko girma |
80 raga | 40% 80 raga (0.17 mm) ko girma |
90 raga | 40% mish (0.15 mm) ko girma |
100 raga | 40% 120 raga (0.12 mm) ko girma |
120 raga | 40% manoma (0.10 mm) ko girma |
150 raga | 40% raga (0.08 mm) ko girma |
180 raga | 40% 250 raga (0.06 mm) ko girma |
220 raga | 40% 270 raga (0.046 mm) ko girma |
Low Chromium: 0.2 zuwa 0.45%
Matsakaici Chromium: 0.45 zuwa 1.0%
Babban chromium: 1.0 zuwa 2.0%
1. Cikakken abu mai rikitarwa, babban wahala da Hardness na kai, kaifi na gefen kai.
2. M, mai wuya, babban matsa lamba resistant, babban abin juriya, a karkashin yanayi na al'ada, bai ƙunshi baƙin ƙarfe ba
3. Tsarin da ya dace da rigar Sandblasting
1 Domin farfajiya na ruwan hoda molten Alumina: mara ƙarfe na fata, kamar yadda ba ƙarfe ba shi da ƙarfe, ban da ƙwayar cuta mai laushi, fenti mai narkewa.
2 LATSA GA FADA: kowane nau'in zinariya, kayan ƙarfe karfe, kayayyakin da ba na gida ba, acrylic da sauran abubuwan da ba hatsi ba, acrylic da sauran kayan aikin ƙasa, na iya haifar da sarrafawa cikin ƙarfe luster.
3. Amfani da etching da sarrafawa: Jade, Dutsen Aya, Semi, Mazauna, Kabilar Marerics, Italiya, Bamobe, da sauransu.
4. Darajar kayan kwalliya, kamar su na dogon-bakin ciki dis dis dis dis dis dis Disc, yankan yankan
5. Gilashin nika na ƙafafun kamar crankshaft nika wheel, kwano niƙa da dabaran, kofin grinding dabaran, da sauransu.
6. Kayan kayan kwalliya, kamar sandpaper da ƙafafun shafa.
7. Haske mai inganci.